A7075铝棒

1/5
A7075铝棒图1

A7075铝棒

¥44.00/公斤
2014-10-15 20:0560询价
参数
  • 重庆西南铝品牌
  • 1公斤起订
  • 湖北产地
湖北 0天内发货 0公斤
产品参数
东莞市尚荣合金制品有限公司普通会员
所在地:湖北
进店逛逛 在线询价
产品详情
A7075铝棒A7075铝棒A7075铝棒A7075铝棒A7075铝棒A7075铝棒A7075铝棒A7075铝棒A7075铝棒A7075铝棒

进口美铝ALCOA7075铝棒哪里有卖? 正宗进口美国ALCOA7075铝棒经销商。

 

7075铝棒简介,AA7075铝棒用途,AL7075铝棒产自美铝

 7075铝棒耐腐蚀铝合金7075已被彻底评估大气风化,应力腐蚀开裂和剥落在目前所有可用的脾气。这些值已被用来作为较近期高的发展比较标准强度航天合金。在7XXX系列合金,抵抗一般攻击,SCC和剥落腐蚀的改善与高峰期相比,显着超龄的脾气(T7启动类型)实力脾气(T6)的。

 
7075铝棒许多热处理和热处理方法可用来谱载下的疲劳裂纹生长行为正在成为日益重要的合金疲劳关键的选择飞机结构。各种高强度航天合金飞行小时的生活中使用两种类型的预测相比,疲劳谱;机翼根应用(张力为主),和水平尾翼的应用(拉伸,压缩)。制定最佳的强度,韧性和其他可取的字符符teristics合金正确应用7075薄板和厚板产品。参照MIL-H6088,铝热处理合金附加信息。
 
Alloy 7075 has been thoroughly evaluated for corrosion resistance,of atmospheric weathering, stress-corrosion cracking and exfoliation,in all currently available tempers. These values have been used as a standard for comparison in the development of more recent high strength aerospace alloys. Within the 7XXX series of alloys,resistance to general corrosion attack, SCC and exfoliation improves significantly in the overage tempers (T7 type) compared with peak strength tempers (T6).
Fatigue crack growth behavior under spectrum loading is becoming increasingly important in the selection of alloys for fatigue critical aircraft structures. Various high strength aerospace alloys are compared for life prediction in flight hours using two types of fatigue spectrums; a wing root application (tension dominated), and a horizontal tail application (tension-compression). develop optimum strength, toughness and other desirable charac- teristics for proper application of alloy 7075 sheet and plate products. Refer to MIL-H-6088, Heat Treatment of Aluminum Alloys for additional information.
 

Alloy 7075 sheet and plate products have application throughout aircraft and aerospace structures where a combination of high strength with moderate toughness 

and corrosion resistance are required.

 

Typical applications are alclad skin sheet, structural plate components up to 4 inches in thickness and general aluminum 

aerospace applications.

 

CHEMICAL COMPOSITION LIMITS (WT. %)

 

Si  . . . . . . . . . . .

0.40

Zn . . . . . . . . . . .

5.1-6.1

Fe . . . . . . . . . . .

0.50

Ti . . . . . . . . . . . .

0.20

Cu . . . . . . . . . . .

1.2-2.0

Others, each . . . .

0.5

Mn . . . . . . . . . . .

0.30

Others, total . . . .

0.15

Mg . . . . . . . . . . .

2.1-2.9

Balance, Aluminum

 

Cr . . . . . . . . . . .

0.18-0.28

 

 

 

Note: value maximum if range not shown.

 
 

 


在线留言

*详情

公司

*姓名

*电话

邮箱

QQ

微信

旺旺

相关公司
相关行业
产品热门搜索
店铺最新
按关键词字母分类:
A B C D E F G H I J K L M N O P Q R S T U V W X Y Z 0-9
A7075铝棒
¥44.00
  • 采购产品
  • 采购数量
  • 联系电话
获取报价
在线问
最近来访记录

    广东省深圳市 鹏博士长城宽带网友 12-09 14:15 用Win10电脑在谷歌浏览器上访问了本页

 
采购 登陆